singlecrystalsuperalloy相关论文
通过改变含Re单晶镍基高温合金热处理过程中的一次时效温度(1150,1180和1200℃),获得了3种不同形貌和尺寸的γ相.随后,对含有不同......
Evolution mechanism of recrystallization in a nickel-based single crystal superalloy under various c
The recrystallization behaviors of a nickel-based single crystal superalloy during heat treatment at 1,200 ℃ for 4 h wi......
An advanced technology for joining powder metallurgy (P/M) superalloy and single crystal (SC) superalloy is highly neede......
小角度偏离[001]取向的镍基单晶高温合金的蠕变性能受温度、γ'尺寸和应力条件的影响.本文综述了镍基单晶高温合金的[001]取向小角......